Coatings Technology Handbook P2

Chia sẻ: A Ly | Ngày: | Loại File: PDF | Số trang:10

0
84
lượt xem
37
download

Coatings Technology Handbook P2

Mô tả tài liệu
  Download Vui lòng tải xuống để xem tài liệu đầy đủ

In the discussion above, high surface tension and low viscosity are required for good flow-out and leveling. But high surface tension can cause cratering, and excessively low viscosity would result in sagging and poor edge coverage. To obtain an optimal coating, the balance between surface tension and viscosity is important. Figure 2.12 illustrates coating performance as a function of surface tension and melt viscosity. Coating is a fairly complex process; achieving an optimal result calls for the consideration of many factors....