Microstructural characteristics of ultra-high performance concrete by grid nanoindentation and statistical analysis

Chia sẻ: _ _ | Ngày: | Loại File: PDF | Số trang:12

2
lượt xem
1
download
 
  Download Vui lòng tải xuống để xem tài liệu đầy đủ

In this study, grid nanoindentation and statistical deconvolution analysis were applied into a developed Ultra-high performance concrete (UHPC) to broaden the understanding of the microstructure phases and their mechanical properties.

Chủ đề:
Lưu

Nội dung Text: Microstructural characteristics of ultra-high performance concrete by grid nanoindentation and statistical analysis