Volume 12 of the 9th Edition of Metals Handbook is the culmination of 43 years of commitment on the part of ASM to the science of fracture studies. It was at the 26th Annual Convention of the Society in October of 1944 that the term "fractography" was first introduced by Carl A. Zapffe, the foremost advocate and practitioner of early microfractography. Since then, the usefulness and importance of this tool have gained wide recognition.