Study of high temperature steam oxidation kinetics during the high temperature oxidation was carried out on the sponge base E110 cladding tubes material in the temperature range 600–1300 °C. The oxidation kinetics derived from the weight gain measurements showed a parabolic rate law for temperatures 1100 °C and higher only.
6p christabelhuynh 30-05-2020 12 1 Download
-
Patients with type 2 vWD have functional defects; thus, the vWF antigen measurement is significantly higher than the test of function. For types 2A, 2B, and 2M, vWF activity is decreased, measured as ristocetin cofactor or collagen binding activity. In type 2A vWD, the impaired function is due either to increased susceptibility to cleavage by ADAMTS13, resulting in loss of intermediate- and high-molecular weight (M.W.) multimers, or to decreased secretion of these multimers by the cell.