This work studies the threshold stress intensity factor (KIH) to initiate DHC as a function of temperature in Zry-4 for temperatures between 227C and 315C. The experimental technique used in this study was the pin-loading testing technique. To determine the KIH, an unloading method was used where the load was successively reduced in a stepwise manner until no cracking was observed during 24 hours.